Making And using A Drawdown Bar - Meyer Rod — Transcript
Full transcript
- 0:02[Music]
- 0:15so I'm asked quite often about coating
- 0:17things because obviously when you laying
- 0:19down a coat and you want repeatability
- 0:21what you need is some method of making
- 0:24sure that the film is the same thickness
- 0:26every time that you put it on now I love
- 0:28the times we just want to do things
- 0:30quickly because we want a sense of stuff
- 0:32in which case things like spray gunning
- 0:34it painting it on with the brush using a
- 0:38roller that sort of stuff
- 0:40it's fine I mean it coats pretty uneven
- 0:42for sure and you can be pretty much
- 0:44guaranteed that from one piece to the
- 0:46next piece the curt is not going to be
- 0:48the same but when you're just testing
- 0:50ideas and you're working through things
- 0:52and you're doing one or two bits of
- 0:54something it really is a fine method
- 0:56when you get closer to what it is that
- 0:59you want to do what you want is some
- 1:00kind of repeatability some way of making
- 1:03sure that that code is the same
- 1:04thickness every time you apply it now
- 1:07there are methodologies of doing this
- 1:09you've got the doctor blade but perhaps
- 1:12the most well used certainly in print
- 1:15and very often in photography for things
- 1:18like albumin coating or gelatin coating
- 1:20that kind of thing is to use what's
- 1:22called the draw down bar now the most
- 1:25popular draw down bar is this which is a
- 1:27Maher rot now the mayor rod is really a
- 1:30stainless steel wrapped piece of steel
- 1:33just interested blank piece of rod and
- 1:35they take a wire of a specific diameter
- 1:37and widened that wire all the way down
- 1:40and what it does is create little cups
- 1:42that are of an even depth all the way
- 1:44and there are standards for this for
- 1:47standard wire thicknesses and standard
- 1:49rug diameters you get for various Maher
- 1:51bars now the principle really is shown
- 1:54in this image
- 2:04and that's pretty much all there is to
- 2:06it so what we're going to do is we're
- 2:09going to show you how to make a mayor
- 2:10rod and then use that mayor rod that
- 2:12we've made to do some drawdown now if
- 2:15you don't feel like making a mayor rod
- 2:17then you can just use some of this stuff
- 2:20this is a threaded bar now it has little
- 2:24rounds in it and obviously it's got a
- 2:26helix so it will lift and create little
- 2:29spots but it does do a good enough job
- 2:31if you don't feel like using a mayor rod
- 2:34and you can get this in different
- 2:35diameters so I think this is an m8 this
- 2:39one's an m12 and you can see I've used
- 2:41this quite often actually and then make
- 2:44pretty decent drawdown bars as well
- 2:46perhaps not the best but certainly
- 2:48pretty decent the mayor rods like I said
- 2:51just a normal bit of Steel this is just
- 2:53mild steel wraps with some stainless
- 2:56steel wire this is a bit of stainless
- 2:58steel rod incidentally which lasts a
- 2:59little bit longer and you make that now
- 3:02the work to make this is like this so to
- 3:06make a mayor rod actually is really easy
- 3:07what I've got here is a bit of bar it's
- 3:09one centimeter mild steel and all I need
- 3:12to do is drill a hole in either end I've
- 3:14put a flat spot on the bar incidentally
- 3:16it just makes it drilling it that much
- 3:18easier the drill doesn't skip off the
- 3:20round surface so put that into a vise
- 3:23and into the drill we can do a couple of
- 3:25holes
- 3:31[Music]
- 3:42holes drilled in it what I've got here
- 3:45is a bit of stainless steel now the only
- 3:47reason I'm using 1 centimeter bar and
- 3:49mr. cendars steel which is point eight 1
- 3:51millimeters incidentally is because it's
- 3:54what I have lying around to be honest
- 3:57you can you so you should use different
- 3:59gauges of stainless steel because the
- 4:02different gauges of the stainless steel
- 4:03will give you different thicknesses of
- 4:05film and we'll go through that when
- 4:07we're actually sat on the desk but to
- 4:08show you how to make the bar are the rod
- 4:11you just feed the stainless steel in a
- 4:13couple of times through the hole that
- 4:14you've just done and pull it tight and
- 4:16that'll be enough to actually make a
- 4:18kind of knot in the end of the steel
- 4:24okay and then twist that round a couple
- 4:27of times and then clip it off obviously
- 4:36I've got a Ledge here and what we're
- 4:39gonna do is wind a coil on the lathe so
- 4:41the bomb goes into the lathe and you're
- 4:46gonna progress it gave me a bit too far
- 4:48out obviously the bar will Bend as you
- 4:50pull on the wire because you have to
- 4:51give it a fair pull to get that thing to
- 4:54work I'll just remove the stock
- 5:06and if I can remember which way around
- 5:08this lid goes so it's turning in that
- 5:20direction pull your wire tight give it a
- 5:28couple of turns by hand just to get it
- 5:31going
- 5:51and when you get close up to this turn
- 5:54it off
- 5:54move it up feed it in and that's all you
- 5:56do so you've gone right to the end your
- 5:58hole is right there incidentally put
- 6:00your thumb on it snip off a fair length
- 6:07and then you want to feed it through the
- 6:09hole at the other end
- 6:40once you've done that Tetsu may rod made
- 6:44incidentally you wind and kiln coils in
- 6:47a similar way to this just get yourself
- 6:48a bar want the coil pull it off stretch
- 6:51it out and it's exactly the same method
- 6:52for winding a kiln coil is for making a
- 6:55mayor rod but there's the mayor rod now
- 6:57let's get back to the desk and use it so
- 6:59once you've made you mayor rod you now
- 7:01have actually a very precise instrument
- 7:03for being able to do film thicknesses
- 7:05but are very very repeatable time and
- 7:08time again those little hills that are
- 7:11formed sink down a little bit and the
- 7:13final finished coat thickness is related
- 7:16to the solid contents of your ink so if
- 7:19you draw down a hundred micrometer thick
- 7:21film and get a 40 percent of solids
- 7:24content what you're going to end up with
- 7:26is a 40 micrometer thick film time after
- 7:30time after time so as long as you know
- 7:32the solid content of your ink the damage
- 7:35of the wire if you bar then your film
- 7:37can be calculated really easily and will
- 7:40be consistent of the entire substrate
- 7:42now obviously when you're laying down
- 7:44the substrate what you need is a flat
- 7:46hard surface and here's a bit of
- 7:48tempered glass that wasn't too expensive
- 7:50actually it was a shelf it's it's a
- 7:52shelf from a cupboard that I got from
- 7:54little local DIY store and get a bit of
- 7:57your substrate
- 7:58just attach it to your shelf or your
- 8:03hard flat surface now I'm going to be
- 8:06using our ink incidentally so I'm gonna
- 8:09put a bit of gloves on just to stop my
- 8:10hands getting too dirty
- 8:24I've hidden the ink another stir just
- 8:27before I use it to make sure we've got
- 8:28good even distribution lay your May
- 8:31around in handy and we'll get a bit of
- 8:35ink ready to go on that
- 8:47put your into cross
- 8:52and then pull the bar down don't roll it
- 9:00and then leave it to dry and you get a
- 9:02beautiful coat on that every time okay
- 9:06so just to run through that one more
- 9:07time a nice flat surface but a tempered
- 9:10glass works really well hard and flat
- 9:12get your substrate whatever that happens
- 9:14to be I'm using this stuff obviously
- 9:16twitch is head to dpe attach that to
- 9:20your flat surface you might use a
- 9:22different material it's totally up to
- 9:24you but I'm using that put the gloves on
- 9:28so I don't get to inky because I'm
- 9:30always washing my hands you may a rod
- 9:37nice and ready
- 9:38remember the thickness of the film is
- 9:40related to the wire diameter is half the
- 9:42wire diameter and then the solid content
- 9:45and you can change that thickness by
- 9:47changing the wire diameter so clearly a
- 9:49larger diameter wire is gonna give you a
- 9:51thicker film a thinner diameter wire
- 9:53will give you a thinner film so changing
- 9:55that wire diameter changes the film
- 9:57thickness but the key of it is its
- 9:59repeatable again and again and again so
- 10:02we've got some ink in our syringe we put
- 10:04a bit of income the substrate
- 10:10don't roll the bar draw the bar so there
- 10:16we go a beautiful coat and here's the
- 10:19one that we did earlier as you can see
- 10:22it's nice and shiny and then we'll leave
- 10:24that to dry properly and that's finished
- 10:26so very easy to do now I did look at the
- 10:30price of these things and they're about
- 10:32two hundred and fifty dollars to buy
- 10:34which I thought was crazy so that's how
- 10:36you go about making one we might
- 10:38actually start making these and selling
- 10:40them on the shop we haven't decided on
- 10:41that or not I guess it depends how much
- 10:43call there is for it really and how much
- 10:44time we have but they're really easy to
- 10:46make at home yourself and they do a
- 10:48beautiful beautiful job so I hope that
- 10:50was of interest to you
- 10:52and thank you very much for watching
About this transcript
This page contains the full transcript of Making And using A Drawdown Bar - Meyer Rod by Robert Murray-Smith, generated from the public captions YouTube serves with the video. The transcript has 1,596 words across 213 segments, with the original timestamps preserved so you can click any line to jump to that moment in the embedded player.
What you can do with it
Use the transcript to take notes, quote the speaker, build a study guide, generate a summary with ChatGPT or Claude via the YouTube Summary tool, or export it as a timed subtitle file with YouTube to SRT. You can also re-open it in the transcriber to choose a caption track available on the video.
Free YouTube transcript tool
YouTube2Text is a free YouTube transcript generator — no signup, no daily limit. Paste any YouTube link and get the full transcript instantly, with timestamps, click-to-jump, caption language selection, AI prompts for ChatGPT, Claude, and Gemini, and exports to TXT, SRT, VTT, or Markdown.